3D-printed conformal cooling channels for injection molds improve productivity
3D Printing3D-printed conformal cooling channels for injection molds improve productivity3D-printed conformal cooling channels for injection molds improve productivity
Conformal cooling technology in injection molds has been around for a couple of decades. It was developed as a way to create cooling channels that follow, or conform, to the shape of the molded part in order to get cooling close to critical areas that otherwise would be difficult to cool, such as thicker wall sections. Conformal cooling technology offers a more uniform way to cool parts, thus reducing cycle time and improving productivity and quality.