3D-printed PEKK stakes out implant position
3D Printing3D-printed PEKK stakes out implant position3D-printed PEKK stakes out implant position
Oxford Performance Materials (OPM), which has been developing polyetherketoneketone (PEKK) as a medical implant plastic, has received FDA 510(k) clearance for its OsteoFab Patient Specific Cranial Device (OPSCD)."OsteoFab" implants are made from PEKK with additive manufacturing technology. According to OPM, it is the first approval for an additively manufactured polymer implant.