Study shows more recycled PET can be used in hot-fill bottles

Study shows more recycled PET can be used in hot-fill bottles

A new study conducted by Plastic Technologies Inc. (PTI; Holland, OH) reveals that the use of recycled polyethylene terephthalate (rPET) in hot-fill packages has no significant adverse impact on the bottles until the blend exceeds 50%.

PTI, which specializes in plastic packaging development, conducted the study to provide information for brand owners contemplating including a percentage of rPET in their hot-fill bottles as part of their environmental initiatives.

“Even at 100% rPET resin use, the performance of the bottle used in this study was still acceptable,” said Tracy Momany, Vice President Product Development Group, PTI. “However, the typically-thicker walls of hot-fill bottles may result in slightly more noticeable haze or yellowing than other applications such as very thin-walled water bottles.”

This study focused on evaluating virgin PET and two different rPET resins added to virgin PET at 25%, 50% and 100% levels. A 27g commercial 500mL six-panel hot-fill bottle and preform were used for the study. Bottles containing recycled-content variables were processed similarly to maintain equivalent bottle wall thicknesses and maximize preform temperatures. The objective was to ensure that the only difference was the amount of recycled content.

PTI tested the bottles to determine hot-fill and top load performance, wall thickness, color, haze, crystallinity and acetaldehyde (AA) content. Following are the main study conclusions:

Results showed that all of samples passed the standard performance specifications for hot fill bottles, even at high percentages of rPET. Also, while shrinkage increased slightly as the recycled content grew above 50%, the bottles remained within the specification.

Drawbacks, according to the company, were increased yellowing and higher haze levels with high rPET content. However, these are aesthetic issues and do not impact performance.

The study proved that converters and brand owners can use up to 50% good quality rPET in hot-fill bottles without negatively impacting performance. rPET levels greater than 50% can also be used, however desired package aesthetics will drive the acceptable level. 

Hide comments
account-default-image

Comments

  • Allowed HTML tags: <em> <strong> <blockquote> <br> <p>

Plain text

  • No HTML tags allowed.
  • Web page addresses and e-mail addresses turn into links automatically.
  • Lines and paragraphs break automatically.
Publish