ISO Certification For Indian OEM A Claimed First

Extruder manufacturer Kolsite, Mumbai, India, has earned ISO 9001:2000 certification from TUV Deutschland, making it the first Indian extruder maker with the recognition, according to the firm. It also says it has sold its first machines in Europe, with the delivery of six compact blown film lines to processor SP Metal Cz, Varnsdorf, Czech Republic.