MaterialsMassive Acrylic Aquarium Bursts in Berlin HotelMassive Acrylic Aquarium Bursts in Berlin Hotel
Only two people were injured as 264,000 gallons of water, some 1,500 exotic fish, and debris gushed through the hotel and into the street.